Polymer Property : Tensile Strength, Yield = 1218 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1218 MPa
176700 psi
Hardened 1900°F, Tempered 1000°F
ATI Allegheny Ludlum 425 Mod Martensitic Stainless Steel
Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for..
Tensile Strength, Yield 1218 MPa

@Strain 0.200 %
176700 psi

@Strain 0.200 %
typical
ATI Allegheny Ludlum Martensitic Stainless Steel Type 425 Mod, Hardened + 538°C Temper
Allegheny Ludlum Type 425 Mod is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stai..