Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 123.8 MPa | 17950 psi | ASTM D638 |
Polymer Resources TP-G20 Polybutylene Terephthalate, 20% Glass Reinforced Polybutylene Terephthalate, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |