Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1270 MPa @Strain 0.200 % |
184000 psi @Strain 0.200 % |
|
Haynes 25 alloy, room temperature after 25% cold reduction Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga.. |
|||
Tensile Strength, Yield | 1270 MPa | 184000 psi | R<sub>p</sub>02. 45 HRC. |
Assab Steels QRO 90 SUPREME Hot Work Steel QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista.. |
|||
Tensile Strength, Yield | 1270 MPa @Strain 0.200 % |
184000 psi @Strain 0.200 % |
|
Haynes 625 alloy, 50% cold reduction Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi.. |