Mechanical Properties Metric English Comments
Tensile Strength, Yield 873 MPa
127000 psi
at Surface, Transverse
International Mold Steel P20 Plastic Mold Steel
P20 tool steel is 28 – 32 HRC (Din # 1.2738). Features better hardenability than AISI P20 due to the addition of nickel. Information provided by International Mold Steel.
Tensile Strength, Yield 873 MPa
127000 psi
at Surface, Longitudinal
International Mold Steel P20 Plastic Mold Steel
P20 tool steel is 28 – 32 HRC (Din # 1.2738). Features better hardenability than AISI P20 due to the addition of nickel. Information provided by International Mold Steel.
Tensile Strength, Yield 873 MPa
127000 psi
at Center, Longitudinal
International Mold Steel P20 Plastic Mold Steel
P20 tool steel is 28 – 32 HRC (Din # 1.2738). Features better hardenability than AISI P20 due to the addition of nickel. Information provided by International Mold Steel.
Tensile Strength, Yield 876 MPa

@Strain 0.200 %
127000 psi

@Strain 0.200 %
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Tensile Strength, Yield 875 MPa

@Strain 0.200 %
127000 psi

@Strain 0.200 %
Precipitation Hardened. Value at room temperature
Special Metals INCONEL® Alloy 751
A nickel-chromium alloy similar to INCONEL ALLOY X-750 but with increased aluminum content for greater precipitation hardening. INCONEL alloy 751 was designed for use as exhaust valves in internal-..
Tensile Strength, Yield 875 MPa

@Strain 0.200 %
127000 psi

@Strain 0.200 %
Precipitation Hardened. Value at room temperature
Special Metals NIMONIC® Alloy 901
A nickel-iron-chromium alloy containing titanium and aluminum for precipitation hardening and molybdenum for solid-solution strengthening. The alloy has high yield strength and creep resistance at ..
Tensile Strength, Yield 876 MPa

@Strain 0.200 %
127000 psi

@Strain 0.200 %
Carpenter Thermo-Span® Fe-Co-Ni Superalloy
Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h..
Tensile Strength, Yield 876 MPa
127000 psi
Long.
ATI Wah Chang 425™ Titanium Alloy, Hot Rolled & Annealed Plate
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..