Polymer Property : Tensile Strength, Yield = 1276 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1276 MPa

@Strain 0.200 %,
Temperature 316 °C
185100 psi

@Strain 0.200 %,
Temperature 601 °F
Carpenter Custom 455® Stainless Steel, Condition H950 (Age Hardened 510°C)
Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope..
Tensile Strength, Yield 1276 MPa

@Strain 0.200 %
185100 psi

@Strain 0.200 %
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition TH 1050
AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va..
Tensile Strength, Yield 1276 MPa
185100 psi
HP Alloys Alloy 718, 5% Cold Worked, Aged
5% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Inte..
Tensile Strength, Yield 1276 MPa
185100 psi
Latrobe Lescalloy® HY-TUF VAC-ARC High Strength Alloy Steel
LESCALLOY HY-TUF VAC-ARC steel is a high strength low alloy steel. It is typically used in the 220/240 ksi (1517/1655 MPa) tensile strength range. At this strength level, the alloy has good ductilit..