Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 8.89 MPa | 1290 psi | ASTM D412 |
Polymax® Maxelast® P1980 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 8.90 MPa | 1290 psi | ASTM D412 |
Precision Polymer Engineering J70P Butyl Rubber Phenolic/Resin cured Butyl Rubber, 65-75 IRHD. Isobutylene-Isoprene Rubber.Applications: Butyl is resistant to the same fluids as Ethylene Propylene (EPDM). It has excellent resistance to gas permea.. |
|||
Tensile Strength, Yield | 8.90 MPa | 1290 psi | 50 mm/min; ASTM D638 |
NOVA Chemicals Novapol® LF-0219-A LDPE Blow Molding Resin Good heat sealing latitude, Easy processabilityApplications: Food contact, Squeeze bottles, Non-ESCRAdditives: Base resinInformation provided by NOVA Chemicals. |
|||
Tensile Strength, Yield | 8.90 MPa | 1290 psi | |
Dow LDPE 722M Low Density Polyethylene DOW LDPE 722M resin is a broad molecular weight distribution homopolymer designed to offer good impact strength and stress crack resistance with excellent flexibility. Typical applications include c.. |
|||
Tensile Strength, Yield | 8.90 MPa @Strain 300 % |
1290 psi @Strain 300 % |
ASTM D412 |
Dow SE BCP 817 Stereospecific high cis-1,4 Polybutadiene (BR) SE BCP 817 is manufactured by a solution process using cobalt catalyst which produces polymers with a very light color and low ash content. A non-staining stabilizer is added during the production .. |
|||
Tensile Strength, Yield | 8.89 MPa | 1290 psi | ASTM D638 |
Clariant Renol PBTSP0006 Polyester Elastomer Data provided by Clariant Masterbatches |