Polymer Property : Tensile Strength, Yield = 13370 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 92.18 MPa
13370 psi
ASTM D638
Mitsui AURUM® PL450C Polyimide  (discontinued **)
AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU..