Polymer Property : Tensile Strength, Yield = 1339.8 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.2376 MPa
1339.8 psi
257°F, 70 hr, in IRM 903 Oil; ASTM D471
ExxonMobil Santoprene® 273-50 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..