Polymer Property : Tensile Strength, Yield = 137.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 137.9 MPa
20000 psi
ASTM D638
PTS Trimid® N6-G30L 30% GFR Lubricated Nylon 6
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 137.9 MPa
20000 psi
ASTM D638
PTS Trimid® N6-G33L 33% GFR Lubricated Nylon 6
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 137.9 MPa
20000 psi
IBC Advanced Alloys Beralcast® 191 Beryllium-Aluminum Alloy
This alloy consists of 65% Be and 35% Al (by weight) and is used primarily for moderate strength cast electronic and thermal packaging applications. BeAl-191 also provides a unique capability for se..