Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 1376 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.487 MPa
1376 psi
160% Retention; Oil Immersion, ASTM #3 oil, 125°C, 7 days
Teknor Apex Flexalloy® 9800-50 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MW Uses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and..