Polymer Property : Tensile Strength, Yield = 1379 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.508 MPa

@Strain 200 %
1379 psi

@Strain 200 %
Saint-Gobain Tygon® S3™ B-44-3 Bio-based Beverage Tubing Formulation
Tygon S3â„¢ B-44-3, from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. The bio-ba..
Tensile Strength, Yield 9.508 MPa

@Strain 200 %
1379 psi

@Strain 200 %
Saint-Gobain Tygon® S3™ B-44-4X Phthalate-free Food, Milk, and Dairy tubing
Tygon S3â„¢ B-44-4X, from Saint-Gobain Performance Plastics, is now phthalate-free. Saint-Gobain is proud to be among the first companies to offer sustainable flexible tubing products. The bio-b..