Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 14.40 MPa | 2088 psi | Change in tensile strength after 168 hours at 212°F; ASTM D638 |
Teknor Apex Sinvicomp SSH 5509 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Flexibility Uses: Cable Jacketing; Wire and Cable Applications Wire Types: ST1; ST2; Type 9; Class 1/3 Agency Ratings: BS 6746; IEC 60502; JIS 6723 Forms: .. |
|||
Tensile Strength, Yield | 14.40 MPa | 2088 psi | Change in tensile strength after 504 hours at 239°F; ASTM D638 |
Teknor Apex Sinvicomp SIH 6007A Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Stiffness Uses: Wire and Cable Applications Wire Types: V-90 Agency Ratings: AS 3147-1992 Forms: Pellets Processing Method: ExtrusionInformation Provided by.. |