Polymer Property : Tensile Strength, Yield = 143 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 0.986 MPa
>= 143 psi
Stress at Elongation M50; ASTM D412 Method A
Seals Eastern 5722 Fluorocarbon-Elastomer
Formulated Viton®. General service.Information provided by Seals Eastern, Inc.