Polymer Property : Tensile Strength, Yield = 143200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 987.3 MPa

@Strain 0.200 %
143200 psi

@Strain 0.200 %
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 30% Cold Work
Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 30% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m..