Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1000 MPa | 145000 psi | |
Pacific Sintered Materials FN-255-S(HT) Nickel Steel Powdered Metal Good impact resistant mechanical components. Good hardenability.Equivalent MPIF Specification: FN-0208-130HTAll information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 1000 MPa @Strain 0.200 % |
145000 psi @Strain 0.200 % |
Typical |
Industeel FORA 360 BC 360 HB Wear Resistant Steel Description: FORA 360 BC is a water quenched, abrasion resistant steel, of a hardness 360 HB. It presents at a good aptitude of implementation in particular in welding.Information provided by manufa.. |
|||
Tensile Strength, Yield | 1000 MPa @Strain 0.200 %, Temperature 650 °C |
145000 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes 718 alloy, cold rolled, solution-treated and aged sheet Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i.. |
|||
Tensile Strength, Yield | 1000 MPa @Strain 0.200 % |
145000 psi @Strain 0.200 % |
|
Haynes Hastelloy® G-30® alloy, 30% cold rolled HASTELLOY® G-30® alloy is a high chromium nickel-base alloy which shows superior corrosion resistance in commercial phosphoric acids as well as many complex environments containing highly oxid.. |
|||
Tensile Strength, Yield | >= 1000 MPa @Strain 0.200 % |
>= 145000 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 50 Austenitic Stainless, Level 4 Cold Worked Cold Worked applies to tensile values and are for 1/4 to 2 in. diameter samples; other properties are typical of this alloy.Nitronic® 50 Stainless Steel provides a combination of corrosion resist.. |
|||
Tensile Strength, Yield | 1000 MPa @Strain 0.200 % |
145000 psi @Strain 0.200 % |
|
Schmolz + Bickenbach MoldMAX HH® High Hard - Copper Alloy Description: Brush Wellman’s MoldMAX HH® (High Hard) is the premier copper mold alloy. This alloy has a hardness and strength comparable with standard tool steels but its thermal conductivit.. |
|||
Tensile Strength, Yield | >= 999 MPa @Strain 0.200 % |
>= 145000 psi @Strain 0.200 % |
|
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), >1.000-1.500 in, STD, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to >1.000-1.500 in, STD, Per Mil-T-9047G; other specific form/thickness entries are also available i.. |
|||
Tensile Strength, Yield | >= 1000 MPa @Strain 0.200 % |
>= 145000 psi @Strain 0.200 % |
|
CLAL-MSX NICLAFOR® 1000 TH4 Quenched/Precipitation Heat Treated, Drawn Copper Alloy Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi.. |
|||
Tensile Strength, Yield | 1000 MPa | 145000 psi | Stress relieved |
California Fine Wire Permanickel® K-300 Nickel Alloy All values may vary dependent on specific design and usagePermanickel® is a registered trade name of the Inco family of products.Capabilities: WireRibbonInsulatedPlatedInformation provided by Calif.. |
|||
Tensile Strength, Yield | 1000 MPa @Strain 0.200 % |
145000 psi @Strain 0.200 % |
|
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition A AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base.. |
|||
Tensile Strength, Yield | 1000 MPa @Strain 0.200 %, Temperature 316 °C |
145000 psi @Strain 0.200 %, Temperature 601 °F |
|
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 900 (Age-Hardened 482°C/1hr/AC) Data provided by Carpenter Technology Corporation.Custom 630 (17Cr-4Ni) is a martensitic precipitation/age-hardening stainless steel offering high strength and hardness along with excellent corrosio.. |
|||
Tensile Strength, Yield | >= 1000 MPa @Strain 0.200 % |
>= 145000 psi @Strain 0.200 % |
|
HP Alloys Nitronic® 60 Austenitic Stainless, Level 4 Cold Worked Level 4 Cold Worked applies to tensile properties of 0.25 to 2 in. sizes; other properties are typical of this alloy.Nitronic 60 is truly an all purpose metal. This fully austenitic alloy was origin.. |