Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 1.01 MPa | >= 147 psi | Stress at Elongation M100; ASTM D412 Method A |
Seals Eastern 7272 Butyl and Halobutyl Rubber General purpose Chlorobutyl; High dampingInformation provided by Seals Eastern, Inc. |
|||
Tensile Strength, Yield | 1.01 MPa | 147 psi | As manufactured |
Unifrax Fiberfrax® 110 Ceramic Fiber Paper 110 paper is a clay-filled, sheeted ceramic fiber paper which is denser and more rigid than other standard grade products. The rigidity is maintained even after burnout of the organic bonding agent.. |