Tensile Strength, Yield 15.1 MPa
2190 psi
ASTM D412
Precision Polymer Engineering V70B Fluoroelastomer Compound
Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene.Applications: Excellent resistance to oils, fuels and hydraulic fluids at high temperature.
Tensile Strength, Yield 15.1 MPa
2190 psi
ISO 527-2
ExxonMobil Exxtral™ BMU 130 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance for automotive exterior applications such as bumper fascia.Availability: Europe F..
Tensile Strength, Yield 15.1 MPa
2190 psi
Molded property
Dow DOWLEX™ 2049 Linear Low Density Polyethylene, Food Grade
DOWLEX® 2049 Polyethylene resin offers excellent tear strength, medium stiffness, outstanding toughness and puncture resistance for films used in food contact applications. When used unmodified and..