Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.865 MPa
2301.0 psi
-5% change after 72 hours @ 250°C; ASTM D412
Precision Polymer Engineering V60D Fluoroelastomer Compound
Fluoroelastomer Rubber, 55-65 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet Aerospace Specifications DTD5612A and DTD5543B Grade 60.Applications: Mouldings which are re..