Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 1030 MPa
>= 150000 psi
Parker Chomerics SPRING-LINE® Beryllium-Copper Gasket
Description: SPRING-LINE beryllium-copper gaskets combine high levels of EMI shielding effectiveness with spring-finger wiping and low closure force properties. The high performance qualities of ber..
Tensile Strength, Yield >= 1030 MPa
>= 150000 psi
Annealed and Aged
IBC Advanced Alloys FA230 Beryllium Nickel Casting Alloy
Beryllium nickel casting alloys are characterized by their steel-like high strength, toughness, and hardness properties. However, unlike the steel alloys, the beryllium nickel alloy system offers th..
Tensile Strength, Yield 1034 - 1207 MPa
150000 - 175100 psi
Materion Beryllium Nickel Strip - Alloy 360 MH6, Mill Hardened
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte..
Tensile Strength, Yield >= 1034 MPa
>= 150000 psi
Materion Beryllium Nickel Strip - Alloy 360 Annealed, 2.5 hr at 950°F
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 2.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation..
Tensile Strength, Yield 1034 - 1340 MPa
150000 - 194000 psi
Materion Beryllium Nickel Strip - Alloy 360 Hard
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 1.2Formability Ratio (bad Way)..
Tensile Strength, Yield >= 1034 MPa

@Strain 0.200 %
>= 150000 psi

@Strain 0.200 %
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), >0.500-1.000 in, STD, Per Mil-T-9047G
Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to >0.500-1.000 in, STD, Per Mil-T-9047G; other specific form/thickness entries are also available i..
Tensile Strength, Yield 1030 MPa

@Strain 0.200 %
150000 psi

@Strain 0.200 %
Aged to ~ 40 HRC
Bohler-Uddeholm UDDEHOLM CORRAX® Precipitation Hardening Stainless Mold Steel
A precipitation hardening stainless steel which offers excellent high corrosion resistance, excellent dimensional stability during hardening and good wear resistance. It can be used at its as-suppli..
Tensile Strength, Yield 1034 MPa

@Strain 0.200 %
150000 psi

@Strain 0.200 %
AK Steel 17-4 PH® Precipitation Hardening Stainless Steel, Condition H 1150
AK Steel 17-4 PH® provides an outstanding combination of high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base..
Tensile Strength, Yield 1034 MPa

@Strain 0.200 %
150000 psi

@Strain 0.200 %
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 25% Cold Reduction
Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good ..
Tensile Strength, Yield 1030 MPa

@Temperature 427 °C
150000 psi

@Temperature 800 °F
ATI Allvac® 718Plus™ Nickel Superalloy
Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the..
Tensile Strength, Yield 1034 MPa

@Strain 0.200 %
150000 psi

@Strain 0.200 %
ATI Allvac® Vasco® Greek Ascoloy Specialty Steel, Heat Treatment: 871°C (1600°F) + Age
Data provided by Allvac.Applications: Compressor blades, vanes, disks, shafts, wheels, fasteners, gas turbine and jet engine components.
Tensile Strength, Yield 1034 MPa

@Strain 0.200 %
150000 psi

@Strain 0.200 %
Carpenter Custom 455® Stainless Steel, Annealed, 1.27 mm Strip
Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope..
Tensile Strength, Yield 1030 MPa
150000 psi
Fully Hardened
ATI Wah Chang Tiadyne™ 3510
Capable of being surface hardened to depths that produce very high wear resistance. Produced by traditional metallurgical processing, not special treatments.Information provided by ATI Wah Chang