Polymer Property : Tensile Strength, Yield = 1540 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 10.6 MPa
1540 psi
100%; ASTM D412
Teknor Apex APEX® 2585-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin..
Tensile Strength, Yield 10.6 MPa
1540 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Laminar Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tensile Strength, Yield 10.6 MPa
1540 psi
Dow DOWLEX™ 2503 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2503 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with excellent rigidity. It h..
Tensile Strength, Yield 10.6 MPa
1540 psi
Dow DOWLEX™ 2503.10 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2503.10 Polyethylene resin is a narrow molecular weight distribution copolymer designed as a superior processing resin. For very thin wall higher cavitation molding, this grade often is a p..
Tensile Strength, Yield 10.6 MPa
1540 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Laminar Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..