Tensile Strength, Yield 1570 MPa
228000 psi
Elgiloy® Co-Cr-Ni Alloy, Strip, 40% Cold Reduction, Heat Treated
Heat Treatment 5 hours at 482°C. The strength, elongation, and hardness values are specific to this heat treatment; other values below are typical of Elgiloy®.General Elgiloy® information: High ..