Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 16.3 MPa | 2360 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G80H Perfluoroelastomer Special, pure white compound with high temperature properties and wide chemical resistance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing p.. |
|||
Tensile Strength, Yield | 16.3 MPa | 2360 psi | ASTM D412 |
Precision Polymer Engineering Z70B Hydrogenated NBR Compound Peroxide cured, Hydrogenated Nitrile Butadiene Rubber (HNBR), 65-75 °IRHD. Medium acrylonitrile content (ACN = 34%). To meet ASTM D2000/SAE J200 line call-out M4DH716, A26, B36, EO16, EO36, F17.A.. |
|||
Tensile Strength, Yield | 16.3 MPa | 2360 psi | ASTM D638 |
ExxonMobil Escorene® LX-0252 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear medium density polyethylene providing an excellent processing window for molding toys and consumer items. The resin is formulated to provi.. |
|||
Tensile Strength, Yield | 16.3 MPa | 2370 psi | |
Spartech M60480 General Purpose PVC First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B.. |
|||
Tensile Strength, Yield | 16.3 MPa | 2360 psi | ASTM D412 |
Teknor Apex APEX® 90-P513A-70-NT Polyvinyl Chloride+PUR Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Forms-PelletsInformation provided by Teknor Apex Company |
|||
Tensile Strength, Yield | 16.3 MPa | 2360 psi | ASTM D638 |
Styron INSPIRE™ TF3800 Polypropylene Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |