Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 16.8 MPa | 2440 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G81H Perfluoroelastomer Special, pure white compound with PTFE blended for improved dynamic performance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties. .. |
|||
Tensile Strength, Yield | 16.8 MPa | 2440 psi | -20% change after 70 hours @ 100°C; ASTM D412 |
Precision Polymer Engineering Q65B Polyurethane Rubber Sulphur cured, Polyurethane Rubber, 55-65 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG621, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resist.. |
|||
Tensile Strength, Yield | 16.8 MPa | 2440 psi | ASTM D412 |
Teknor Apex APEX® 3210-90 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Sterilizable, Radiation Uses-Automotive Applications, Connectors, Non-specific Food Applications, Ge.. |
|||
Tensile Strength, Yield | 16.8 MPa | 2430 psi | Change in tensile strength after 168 hours at 176°F; ASTM D638 |
Teknor Apex Sinvicomp SIG 5001 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Stiffness Uses: Electronic Insulation; Wire and Cable Applications Wire Types: C; D; TI2; YI2; T11; Y11 Agency Ratings: BS 6746; IEC 60227; VDE 0207 Forms: .. |
|||
Tensile Strength, Yield | 16.8 MPa | 2430 psi | Change in tensile strength after 168 hours at 176°F; ASTM D638 |
Teknor Apex Sinvicomp SIG 5062 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: High Stiffness Uses: Electronic Insulation; Wire and Cable Applications Wire Types: C; D; TI2; YI2; T11; Y11 Agency Ratings: BS 6746; IEC 60227; VDE 0207 Forms: .. |
|||
Tensile Strength, Yield | 16.8 MPa | 2440 psi | ASTM D412 |
Vicone High Performance Rubber VicoSeal™ 617N-BK High Performance EPDM Rubber Two Material Product:Material 1: VicoSeal™ 617N-70 DUROMaterial 2: SS304 nitrile vulcanized to SS304 (RoHS Approved)Information provided by Vicone |
|||
Tensile Strength, Yield | 16.8 MPa | 2430 psi | Change in tensile strength after 168 hours at 212°F; ASTM D638 |
Teknor Apex Sinvicomp SIH 5009 Polyvinyl Chloride, Flexible Availability: Asia Pacific Features: Good Stiffness Uses: Electronic Insulation; Wire and Cable Applications Wire Types: A; B; YI4; YI5 Agency Ratings: IEC 60502; VDE 0207 Forms: Pellets Processing .. |
|||
Tensile Strength, Yield | 16.8 MPa | 2440 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® SMR1555 Thermoplastic Polyolefin Elastomer Elastocon® SMR1555 thermoplastic polyolefin elastomer has been developed for applications that require low temperature impact resistance and a high gloss scratch and mar resistant surface finish. E.. |