Polymer Property : Tensile Strength, Yield = 164 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 164 MPa
23800 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Nymax™ NM 6600-44GF0001 White Polyamide 66 (Nylon 66)
The Nymax® GMF 1200 Series of compounds are based upon nylon 6/6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part per..
Tensile Strength, Yield 164 MPa
23800 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-KON REL33 PA 66
LNP STAT-KON* REL33 is a compound based on Nylon 66 resin containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant.
Tensile Strength, Yield 164 MPa
23800 psi
ASTM D638
Ashley Polymers Ashlene® 980LS-33G Nylon 612, 33% Glass Reinforced
A 33% glass reinforced, heat stabilized Nylon 612 resin.Data provided by the manufacturer
Tensile Strength, Yield 164 MPa

@Strain 0.200 %,
Temperature 593 °C
23800 psi

@Strain 0.200 %,
Temperature 1100 °F
0.059" Coil
AK Steel 15 Cr-Cb® ULTRA FORM® Ferritic Stainless steel
AK Steel’s 15 Cr-Cb ULTRA FORM® is a low-carbon, low-nitrogen ferritic grade of stainless steel with an intermediate, 14.5% chromium content. Alloying additions of Ti, Cb, Si and Mn provide excell..