Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 11.4 MPa | 1660 psi | AVG Stress at Elongation M50; ASTM D412 Method A |
Seals Eastern 7182B Fluorocarbon-Elastomer Formulated AFLAS® high-temperature, high-pressure "sour" oil & gas service. ED resistant. Excellent acid and base resistance.Information provided by Seals Eastern, Inc. |