Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1150 MPa @Strain 0.200 % |
167000 psi @Strain 0.200 % |
|
Haynes 188 alloy, 30% cold reduction, 3.2 mm thick sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Tensile Strength, Yield | 1150 - 1300 MPa @Strain 0.200 % |
167000 - 189000 psi @Strain 0.200 % |
|
SSAB Tunnplat Docol® 1400 DP High-strength Steel The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is the next stage, in which the steel .. |
|||
Tensile Strength, Yield | 1150 MPa @Strain 0.200 % |
167000 psi @Strain 0.200 % |
|
Bisalloy Steels BisPlate 450 Thickness 8-20 mm A through hardened, abrasion resistant steel plate, with guaranteed high impact toughnessApplications: Dump Truck Bodies, Mining Buckets, Tipper Bodies, Cutting Edges, Dump Truck Wear Liners, Constr.. |