Polymer Property : Tensile Strength, Yield = 17.08 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.08 MPa
2477 psi
22% change after 72 hours @ 250°C; ASTM D412
Precision Polymer Engineering Perlast® G71H Perfluoroelastomer
Special, white compound, with PTFE blended for improved dynamic performance. Has excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties. Appl..