Mechanical Properties Metric English Comments
Tensile Strength, Yield 1710 MPa

@Strain 0.200 %,
Temperature 204 °C
248000 psi

@Strain 0.200 %,
Temperature 399 °F
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 53%, Aged 565°C/4hr/AC
Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good ..
Tensile Strength, Yield 1710 MPa
248000 psi
HP Alloys Alloy 718, 50% Cold Worked, Aged
50% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int..