Mechanical Properties Metric English Comments
Tensile Strength, Yield 173 MPa
25100 psi
ISO 527-2/1A/5
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot..
Tensile Strength, Yield 173 MPa
25100 psi
5 mm/min, Type 1A; ISO 527-2
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
AV-755 SL45 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like th..
Tensile Strength, Yield 173 MPa
25100 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Stat-kon REL36 PA 66
LNP* Stat-Kon* REL36 is a compound based on Nylon 6/6 containing carbon fiber and PTFE. Characteristics of this grade are Statically Conductive.This data was supplied by SABIC-IP for the Americas r..
Tensile Strength, Yield 173 MPa
25100 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP QCP36 PA6.10
LNP* LUBRICOMP* QCP36 is a compound based on Nylon 6/10 resin containing 15% PTFE/Silicone, 30% Carbon Fiber. Added features of this material include: Wear Resistant. Electrically Conductive
Tensile Strength, Yield 173 MPa
25100 psi
ASTM D638
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66
LNP* STAT-KON* REF42 is a compound based on Nylon 66 resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
Tensile Strength, Yield 173 MPa
25100 psi
ASTM D638
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 (Asia Pacific)
LNP* Stat-kon* REF42 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Fiber.
Tensile Strength, Yield 173 MPa
25100 psi
ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP QCP36 PA 6/10 (Asia Pacific)
LNP* Lubricomp* QCP36 is a compound based on Nylon 6/10 resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conducti..