Polymer Property : Tensile Strength, Yield = 1769 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 12.20 MPa
1769 psi
ISO 527-2
Borealis Borcellâ„¢ LE1120 Low Density Polyethylene for Physically Foamed Cellular Insulation
Borcell LE1120 is a low density polyethylene intended for the insulation of coaxial and radio frequency communication cables.. It contains no additives and is designed to give the lowest possible a..