Polymer Property : Tensile Strength, Yield = 1820 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1820 MPa
264000 psi
R<sub>p</sub>02. 56 HRC.
Assab Steels HOTVAR Hot Work Steel
HOTVAR is a high performance molybdenum-vanadium alloyed hot-work tool steel which is characterized by:High hot wear resistanceVery good high temperature propertiesHigh resistance to thermal fatigue..