Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1282 MPa @Strain 0.200 %, Temperature 204 °C |
185900 psi @Strain 0.200 %, Temperature 399 °F |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, Cold Drawn 33%, Aged 565°C/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |