Polymer Property : Tensile Strength, Yield = 19.73 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.73 MPa
2861 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 93A
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tensile Strength, Yield 19.73 MPa
2861 psi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 93A
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..