Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1900 MPa | 276000 psi | 0° |
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Strength 12k carbon UD tape supported S25 150 g/m2 Information provided by HexCel |
|||
Tensile Strength, Yield | 1900 MPa | 276000 psi | |
Elgiloy® Co-Cr-Ni Alloy, Wire, 47% Cold Reduction (Coil Spring Range), Heat Treated Heat Treatment 5 hours at 527°C. 45-48% cold reduction is the normal coil spring range. The strength, shear modulus, and hardness values are specific to this heat treatment; other values below ar.. |
|||
Tensile Strength, Yield | 1900 MPa @Strain 0.200 % |
276000 psi @Strain 0.200 % |
|
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 538°C (1000°F) Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati.. |
|||
Tensile Strength, Yield | 1900 MPa | 275000 psi | |
Carpenter AerMet® 310 AerMet 310 alloy possesses higher hardness and strength than AerMet 100 alloy while maintaining exceptional ductility and toughness. At a 310 ksi (2137 MPa) ultimate tensile strength, AerMet 310 all.. |