Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 132 MPa | 19200 psi | ASTM D638 |
Techmer ES Luriblend® PPS GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 132 MPa | 19200 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® AR-5300H PBT/ASA, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 132 MPa | 19200 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® AR-5300H PBT/ASA, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 132 MPa | 19200 psi | ASTM D638 |
Samyang Tribit® 1500G30 Polybutylene Terephthalate, 30% Glass Reinforced Characteristics:G/F reinforcedHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll infor.. |
|||
Tensile Strength, Yield | 132 MPa | 19200 psi | ASTM D638 |
Cheng Yu Plastic NG1250S Nylon 66, 25% Glass Fiber Reinforced |