Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 13.31 MPa | 1930 psi | 10% change after 72 hours @ 250°C; ASTM D412 |
Precision Polymer Engineering V75B Fluoroelastomer Compound Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out: M2HK710, A1-10, B37, B38, EF31, EO78, F14, Z1, where Z1 = compressi.. |
|||
Tensile Strength, Yield | 13.3 MPa | 1930 psi | ASTM D412 |
Teknor Apex APEX® 3300-70 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses-Food Service Applications, Medical Applications, TubingAppearance-ClearForms-PelletsProcessing-Extrusio.. |
|||
Tensile Strength, Yield | 13.3 MPa | 1930 psi | after aging 1 week @ 135°C; ASTM D638 |
Trelleborg Horda Cable E8409 Easy Strippable Semiconductive Shielding E8409 is a vulcanizable, strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes.E8409 meets the requirements as be.. |
|||
Tensile Strength, Yield | 13.3 MPa @Strain 100 % |
1930 psi @Strain 100 % |
ASTM D638 |
Toyobo E1095A Thermoplastic Polyurethane Elastomer, Extrusion Grade Polybutyleneadipate type, the most general purpose type of Toyobo Polyurethane; features excellent cost-performance. Various grades of Toyobo polyurethane TPEs are used in auto parts, hoses, tubes,.. |