Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1370 MPa @Strain 0.200 % |
199000 psi @Strain 0.200 % |
|
QuesTek® Innovations Ferrium® C64™ Case-hardened Gear Steel with Ultrahigh-strength Core Description: Ferrium® C64™ is a member of a new class of martensitic secondary-hardening gear and bearing steels that utilize an efficient M2C precipitate strengthening dispersion. Because of the .. |
|||
Tensile Strength, Yield | 1372 MPa @Strain 0.200 %, Temperature 260 °C |
199000 psi @Strain 0.200 %, Temperature 500 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |