Polymer Property : Tensile Strength, Yield = 2.65 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2.65 MPa
384 psi
ASTM D412
Polymax® Maxelast® P2625 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 2.65 MPa
384 psi
ASTM D412
Polymax® Maxelast® P2740 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Strength, Yield 2.65 MPa
384 psi
@100% Elongation; ASTM D1414
Greene Tweed CHEMRAZ® 656 Perfluoroelastomer
Chemraz® 656 is a low durometer perfluoroelastomer primarily designed for Bonded Slit Valve gates and special engineered applications such as low sealing forces/tolerance stickups where softer ma..
Tensile Strength, Yield 2.65 MPa

@Strain 100 %
384 psi

@Strain 100 %
ASTM D412
Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based
Data provided by Clariant Masterbatches