Tensile Strength, Yield 11.7 - 200 MPa
1700 - 29000 psi
Average value: 27.9 MPa Grade Count:339
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Tensile Strength, Yield 112 - 200 MPa
16200 - 29000 psi
Average value: 171 MPa Grade Count:12
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Tensile Strength, Yield 108 - 200 MPa
15700 - 29000 psi
Average value: 133 MPa Grade Count:4
Overview of materials for Nylon 612, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of..
Tensile Strength, Yield 82.7 - 200 MPa
12000 - 29000 psi
0.2% offset
Eagle Brass 240 Low Brass, Annealed
CDA 240 has excellent ductility, corrosion resistance and strength which allows it to be deep drawn, etched, stamped, blanked and bent. Typical uses include musical instruments, battery caps, flexib..
Tensile Strength, Yield 131 - 200 MPa
19000 - 29000 psi
0.2% offset
Eagle Brass 510 Phosphor Bronzes 5% A, Annealed
Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info..
Tensile Strength, Yield 160 - 200 MPa
23200 - 29000 psi
ArcelorMittal 04 High formability steel for drawing, Cold rolled
Available in the following: uncoated (DC04) and electroglavanized (DC04+ZE) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These product..
Tensile Strength, Yield 160 - 200 MPa
23200 - 29000 psi
ArcelorMittal 54 High formability steel for drawing, Cold rolled
Available in the following: Extragal®/Galvannealed (DX54D +Z/+ZF)Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used..
Tensile Strength, Yield 13.0 - 200 MPa
1890 - 29000 psi
Average value: 26.3 MPa Grade Count:86
Overview of materials for High Density Polyethylene (HDPE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Extruded". Each property range of values reported is minimum and maxim..