Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 15.00 MPa | 2175 psi | ISO 527 |
MRC Polymers MAXTELâ„¢ 600T25 TPO, 25% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Tensile Strength, Yield | 15.00 MPa | 2175 psi | ASTM D-638 |
Axiall 18760 Wire & Cable Flexible PVC Non-lead stabilized, matte-finish, jacketing compound with excellent low temperature performance. Maximum 105°C service temperature at 40+ mil. Ideally suited for 90°C applications.Information p.. |