Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 150.00 MPa | 21755 psi | ASTM D638 |
Fiberfil® FPI-33 BK Nylon 6, 33% Glass Reinforced, post industrial Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 150.00 MPa | 21755 psi | ASTM D638 |
Fiberfil® FV-30 Nylon 6, 30% Glass Reinforced, Heat Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 150.00 MPa | 21755 psi | ASTM D638 |
Fiberfil® FV-31 Nylon 6, 31% Glass Reinforced, Heat Stabilized Information provided by FIBERFIL Engineered Plastics |