Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 68.9 - 150 MPa | 10000 - 21800 psi | Average value: 106 MPa Grade Count:37 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Tensile Strength, Yield | 130 - 150 MPa | 18900 - 21800 psi | Average value: 141 MPa Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Tensile Strength, Yield | 16.5 - 150 MPa | 2400 - 21800 psi | Average value: 111 MPa Grade Count:7 |
Overview of materials for Polypropylene with 60% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i.. |