Tensile Strength, Yield 15.138 MPa
2195.6 psi
-13% change after 72 hours @ 250°C; ASTM D412
Precision Polymer Engineering Perlast® G70T Perfluoroelastomer
A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require long-ter..