Polymer Property : Tensile Strength, Yield = 2221 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 2221 MPa
322100 psi
Typical epoxy composite property
Hexcel® HexTow™ AS4 Carbon Fiber
HexTow™ AS4 carbon fiber is a continuous, high strength, high strain, PAN based fiber available in 3,000 (3K), 6,000 (6K), and 12,000 (12K) filament count tows. The fiber has been surface treated a..