Polymer Property : Tensile Strength, Yield = 225100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1552 MPa

@Temperature 24.0 °C
225100 psi

@Temperature 75.2 °F
Hexcel® HexPly® F155 Epoxy Resin, T3T095 Carbon Tape
Hexcel designation: TXX095-12"-F155; Various fibersInformation provided by HexCel
Tensile Strength, Yield 1552 MPa

@Strain 0.200 %
225100 psi

@Strain 0.200 %
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition RH 950
AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala..