Tensile Strength, Yield 231 - 240 MPa

@Temperature -40.0 - -40.0 °C
33500 - 34800 psi

@Temperature -40.0 - -40.0 °F
Average value: 236 MPa Grade Count:2
Overview of materials for Nylon 66, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Tensile Strength, Yield 231 MPa
33500 psi
ASTM D638
Techmer ES HiFill® PA4/6 GF45 HS BK 45% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 45% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackTPCI# 9627150Informat..
Tensile Strength, Yield 231 MPa
33500 psi
ASTM D638
Techmer ES HiFill® PA6 GF60 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Tensile Strength, Yield 231 MPa
33500 psi
ASTM D638
Techmer ES HiFill® PA6 GF60 HS L 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati..
Tensile Strength, Yield 231 MPa
33500 psi
ASTM D638
Techmer ES HiFill® PA6 GF60 HS L BK 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackProcessing Method: In..