Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 16.12 MPa | 2338 psi | 12 hours post cure |
ACC SMP™ EP 82 EPI Engineered Polymers Silicone Modified Polyurea EP 82, “Powered by Reactamine® Technology”, is a new hydrophobic silicone polyurea. The product is characterized by its low viscosity and ability to readily blend with polyisocyanates. It may be .. |