Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 16.4 MPa | 2380 psi | ASTM D412 |
Teknor Apex Flexalloy® 9300-70 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R.. |