Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 242 MPa | 35100 psi | ASTM D638 |
LNP Thermocomp® UF-1009 HS Polyphthalamide, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Tensile Strength, Yield | 242 MPa | 35100 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK LNP* THERMOCOMP* LC008E is a compound based on Polyetheretherketone resin containing 40% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Tensile Strength, Yield | 242 MPa | 35100 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP LC008E PEEK (Asia Pacific) LNP* Thermocomp* LC008E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |