Polymer Property : Tensile Strength, Yield = 245000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 1690 MPa

@Strain 0.200 %
245000 psi

@Strain 0.200 %
ATI Allvac® VascoMax® C-250 Specialty Steel, Heat Treatment: 927°C (1700°F) + Age
Data provided by Allvac.Applications: Missile components, tooling and other applications requiring good toughness with high strength. Jet engine shafts.